Suppressing Reductive Deactivation of Fe 2 O 3 via In─O─Fe Motif Formation for CO 2 Hydrogenation

View at publisher
Authors: Huayu Gu, Bing Zhu, Yuanyuan Wang, Okkyun Seo, Ziyang Toh, Daiju Mastumura, Jiayi Tang, Fanfei Sun, Dongshuang Wu
Cited by: 3
References: 56

Abstract

ABSTRACT Transition‐metal oxides are susceptible to over‐reduction under hydrogen‐rich conditions, thereby hindering intermediate turnover and accelerating deactivation. Embracing this reaction reality, we show that Fe 2 O 3 inevitably converts to Fe 3 O 4 during reverse water‐gas shift (RWGS) at 300°C, yet can be reactivated by forming interfacial In─O─Fe motifs through in situ oxidation of indium (In). Operando and post‐reaction analyses identify In 2 O 3 /Fe 3 O 4 as the working architecture. At these interfaces, strong sp–sp orbital hybridization between In and O atoms weakens the C─O bond within surface formate and accelerates its decomposition, shortening its surface residence and leading to high stability. In contrast, Fe─O─C orbital conjugation in Fe 3 O 4 reinforces electronic delocalization, thereby stabilizing the intermediate and poisoning the surface. The In‐modified catalyst delivers nearly twofold higher CO yield than Fe 2 O 3 and exhibits marked durability at 450°C (activity loss 6% versus 62%). Rather than preventing phase transformation by bulk lattice stabilization (e.g., doping heteroatoms/constructing high‐entropy oxides), this interface‐motif strategy rebuilds functionality on the reduced steady state of transition metal oxides, providing a concise route to durable CO 2 hydrogenation.

Fields of Study & Subjects

Catalysts for Methane Reforming Catalytic Processes in Materials Science Catalysis for Biomass Conversion

Publication details

Journal / source
Angewandte Chemie International Edition
Publisher
Wiley
Volume
65
Issue
16
Pages
e4720181–e4720181
Publication date
1 March 2026
Language
EN