Influence of temperature and pressing time on the properties of medium density fiberboards made from Pinus taeda L.

Read full text
Authors: Alexsandro Bayestorff da Cunha, Joelson Lima Ferreira, Tarcisio Francisco de Camargo, Rodrigo Figueiredo Terezo, Camila Alves Corrêa, Natalia Durigon Melo, Martha Andréia Brand, Polliana D’Angelo Rios
Cited by: 1
References: 27

Abstract

The study’s objective was to evaluate the pressing stage of medium-density fiberboards made of Pinus taeda , which has a thickness of 15 and 18 mm and is influenced by temperature and pressing time on the physical and mechanical properties. The methodology was divided into two stages: (i) evaluation of the temperature in the center of the panels until the adhesive cured (100 °C), plus an additional 10 min; (ii) evaluation of the properties of the panels over each minute after reaching the minimum adhesive curing time. As a result, five distinct temperature phases were observed in the center of the panel, where we can highlight the rapid increase in the variable in the second phase, a plateau stage in the fourth phase, and the resumption of the temperature in the last phase; and; minimum pressing times to meet the parameters of the reference standard of 5:18 min for a thickness of 15 mm and 6:52 min for 18 mm.

Fields of Study & Subjects

Natural Fiber Reinforced Composites Wood Treatment and Properties activated carbon and charcoal

Publication details

Journal / source
Journal of the Indian Academy of Wood Science
Publisher
Springer Science and Business Media LLC
Volume
23
Issue
1
Pages
49–59
Publication date
2 May 2026