Coke-resistant Ni/Al2O3 catalysts for low-temperature dry reforming of methane via Ni0/NiAl2O4 interface control

Read full text
Authors: Wenzheng Zhang, Ouardia Akdim, Nan Zhang, Xueping Deng, Huahua Zhao, Jian Yang, Huanling Song, Yongfeng Hu, Lingjun Chou, Graham J. Hutchings
Cited by: 4
References: 39

Abstract

The dry reforming of methane (DRM) is a key process for valorizing CO 2 and CH 4 , yet the catalyst longevity is limited by severe coking at low temperature. Among various catalysts studied, NiAl-based systems have been a long-standing research focus due to their inherent advantages. However, their practical application has been perpetually hampered by vulnerability to coke formation. This study investigates the effect of varying the Ni 0 /Ni 2+ ratio (from NiAl 2 O 4 ) in a 5 wt.% Ni/Al 2 O 3 catalyst, while controlling particle size and Ni dispersion, on coke resistance under conditions where carbon formation is thermodynamically favored, i.e., 600 o C, CH 4 :CO 2 :N 2 = 25:25:10, GHSV = 150 L g cat -1 h -1 . Using in situ XANES, we established that a catalyst formulation, Ni 0 /NiAl 2 O 4 /Al 2 O 3 , with 32.5% Ni 0 and 67.5% Ni 2+ achieves the highest performance. Comprehensive pulse experiments and in situ diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS) provides insights into the reaction mechanism, wherein CH x * (* adsorbed) species from CH 4 dissociation on Ni 0 are rapidly oxidized by the surface O* from NiAl 2 O 4 to form HCO 3 * and CO 3 * intermediates. Simultaneously, the CO disproportionation route to coke is suppressed. In contrast, a catalyst lacking this optimized interface readily promotes coke deposition.

Fields of Study & Subjects

Catalysts for Methane Reforming Zeolite Catalysis and Synthesis Catalysis for Biomass Conversion

Publication details

Journal / source
Applied Catalysis B: Environmental
Publisher
Elsevier BV
Volume
391
Pages
126705–126705
Publication date
21 March 2026
Language