Abstract

Abstract In this paper, for the electron beam weldments of TC11 and Ti-22Al-25Nb, the evolution of microstructures in fusion zone and heat affected zone as well as the changes in mechanical properties are investigated through isothermal forging deformation and subsequent heat treatment effects. The results show that the weld fusion zone of the two alloys after vacuum electron beam welding is mainly composed of β phase, the microstructure of the heat-affected zone of TC11 alloy is composed of α, α’ and β phase, and the heat affected zone of Ti-22Al-25Nb alloy is mainly composed of α 2 and B2 phase. After isothermal forging deformation and heat treatment, fine O phase was precipitated in the weld fusion zone. There are primary equiaxial α 2 phases in the weld fusion region after 940°Cdeformation and heat treatment. The fusion zone is weak region in the tensile process, and fracture occurs in this region. The precipitation of the phase makes the tensile strength of the fusion region improved. The tensile strength of the dual-alloy specimen in the welded state is low, only 934 MPa, while the elongation is 6.5%. The tensile strength of the weld fusion zone is increased by thermal action, such as after 980 ° C, 0.001s −1 , 40% deformation and heat treatment, the room temperature tensile strength of the joints is increased by 21.2% compared to the welded state, reaching 1132 MPa. The impact toughness of the weld fusion zone of the weldments is the largest in the welded state, reaching 18.8 J·cm −2 . With the applied heat and force, the plasticity decreased due to the precipitation of reinforcing phases, resulting in a decrease in the impact value of the weld down to 6.9 J·cm −2 after 940 ° C, 0.001s −1 , 40% deformation and heat treatment.

Fields of Study & Subjects

Advanced Welding Techniques Analysis Titanium Alloys Microstructure and Properties Intermetallics and Advanced Alloy Properties

Publication details

Journal / source
Journal of Physics Conference Series
Volume
3182
Issue
1
Pages
012001–012001
Publication date
1 March 2026
Language
EN