Identification of inclusion sources by slag tracers during the ladle change operation

Read full text
Authors: Christoph Truschner, Sergiu Ilie, Alfred Jungreithmeier, Susanne Michelic
Cited by: 0
References: 62

Abstract

The cleanness of steel is significantly influenced by the casting conditions during continuous slab casting. Unsteady casting conditions, such as those occurring during a ladle change, may deteriorate the cleanness of the cast product but are process-wise unavoidable. This study investigates the impact of ladle change operation on meso- and macroscopic cleanness levels and seeks to uncover the origin of these non-metallic inclusions (NMIs). To facilitate the identification of the particles’ source, slag tracers were employed to mark ladle and tundish slag. Hot-rolled coils produced from slabs cast during the ladle change were sampled along their entire length and characterised for meso- and macro-NMIs. The inclusions’ positions were then projected to the corresponding positions within the initial strand. The ladle change event significantly deteriorated the strand's meso- and macro-cleanness over a total casting length of approximately 19 m. During the period, as the tundish weight decreased, the largest inclusions were detected. The highest concentration of meso- and macro-NMIs was observed shortly before the start of casting of the subsequent heat. The following sources for meso- and macroscopic NMIs were determined during the ladle change: ladle slag, mould slag and eroded refractory material.

Fields of Study & Subjects

Metallurgical Processes and Thermodynamics Iron and Steelmaking Processes Materials Engineering and Processing

Publication details

Journal / source
Ironmaking & Steelmaking Processes Products and Applications
Publication date
3 February 2026
Language
EN