SELECTION OF MODIFIERS FOR HIGH-MANGANESE STEEL DEPENDING ON THE OPERATING CONDITIONS OF MINING AND PROCESSING EQUIPMENT COMPONENTS
Summary
No summary yet. VIRAT can read this paper and write a plain-language summary of its aim, methods, key findings and limitations.
Summarise with VIRAT Free to try with your Science Catalogs account.Abstract
Purpose. To establish the optimal modifier for increasing the strength and ductility properties of high-manganese Hadfield steel, as well as wear resistance during dry and wet grinding in an alkaline environment. Research methods. Impact and abrasive wear resistance tests during wet and dry grinding were carried out in a ball mill. Tensile tests were carried out on a URM-50 machine. Determination of the impact strength of samples with a U-shaped notch was carried out on a pendulum impactor MK-30A according to DSTU ISO 148-1:2022. Brinell hardness was determined according to DSTU ISO 6506-1:2007. Results. Based on the results of experimental studies, it was found that the optimal way to increase the physical and mechanical properties and wear resistance of high-manganese steel during dry grinding is a complex modification with titanium and vanadium with preliminary deoxidation with aluminum. The optimal technological factor that increases the wear resistance of high-manganese steel parts during wet grinding in an alkaline environment is the modification of the melt with 0.05 ... 0.15% Nb with preliminary deoxidation with aluminum. Scientific novelty. In steel modified with aluminum, film nitrides of aluminum were found, around which, apparently, corrosion destruction occurs. When modifying Nb within 0.06–0.12 %, film nitrides are practically absent. The bulk of the inclusions were complex nitrides of aluminum and niobium, as well as carbonitrides of niobium. The effect of niobium on wear resistance is positive and during wet grinding has a pronounced extreme character with an optimum at a content of 0.12% Nb. Practical value. An optimal method for improving the physical and mechanical properties and wear resistance of high-manganese steel during dry grinding has been identified: complex modification with titanium and vanadium followed by aluminum deoxidation. The optimal process factor for increasing the wear resistance of high-manganese steel components during wet grinding in an alkaline environment is niobium modification of the melt. The proposed recommendations will reduce the material intensity of mining and processing equipment, improve production, and increase the reliability and durability of high-manganese steel components.
Fields of Study & Subjects
Metal Alloys Wear and Properties
Microstructure and Mechanical Properties of Steels
Metallurgical Processes and Thermodynamics
Publication details
- Journal / source
- New Materials and Technologies in Metallurgy and Mechanical Engineering
- Issue
- 1
- Pages
- 6–15
- Publication date
- 31 March 2026
- Language
- EN