INFLUENCE OF STRUCTURAL FACTOR OF POWDER MATERIAL ON ELEMENTS STRENGTH
Summary
No summary yet. VIRAT can read this paper and write a plain-language summary of its aim, methods, key findings and limitations.
Summarise with VIRAT Free to try with your Science Catalogs account.Abstract
Purpose. To investigate the influence of porosity and chemical composition on the strength of titanium structural components made from the unalloyed titanium alloy VT1-0, manufactured by powder metallurgy. The work aims to refine the methodology for calculating such components while taking into account the specific features of their structure, since the presence of pores contradicts the traditional hypothesis of material continuity. Research methods. For the experiment, thermomechanical titanium powder PT5 was used. After pressing (700 MPa) and vacuum sintering (1250 °C, 180 min), the VT1-0 alloy was obtained. A comparative analysis of the structure and mechanical properties of the sintered material and its cast counterpart was carried out. Results. The key structural distinction is the porosity of the sintered alloy, which is 13 %, with pores located mainly along grain boundaries. In terms of chem-ical composition, powder-based VT1-0 has twice the oxygen content (0.20 wt%) compared to the cast alloy (0.10 wt%). It is known that oxygen significantly increases the strength of titanium alloys; however, the ultimate strength of the sintered VT1-0 alloy was 330.5 MPa, which is 45.5 MPa lower than that of its cast counterpart (376.0 MPa). This is due to the presence of pores in the metal structure. Eliminating these pores will increase strength compared to a cast material of similar chemical composition and reduce its dispersion to that of a cast alloy. Scientific novelty. The main conclusion of the study is that the reduction of the effective metal cross-section bearing the load (due to 13 % porosity) outweighs the strengthening effect of the higher oxygen and other substance’s content. The presence of pores also leads to a significant increase in the scatter of strength and in some cases microhardness values. If we make a correction for the effective cross-sectional area minus the pores, the actual strength of the powder sample would be higher due to the increased oxygen and other substance’s content. Practical value. It was proved that the actual negative effect of porosity on strength is significantly outweighed by the strengthening effect resulting from microalloying with impurities during sintering. Given the high dispersion of the strength index, this effect can be explained by the fact that the influence of porosity on the ultimate strength is multidimensional and depends on factors such as pore shape and size, the presence of sharp corners in them and their volume fraction.
Fields of Study & Subjects
Powder Metallurgy Techniques and Materials
Titanium Alloys Microstructure and Properties
Cellular and Composite Structures
Publication details
- Journal / source
- New Materials and Technologies in Metallurgy and Mechanical Engineering
- Issue
- 1
- Pages
- 24–30
- Publication date
- 31 March 2026
- Language
- EN