ENHANCING THE QUALITY OF KAOLIN FEEDSTOCK VIA ELECTROLYTIC REMOVAL OF FERRUGINOUS INCLUSIONS

Read full text Summarise with VIRAT
Authors: Іhor Piskun, Volodymyr Kotenko, Ярослав Олегович Наумов, Mykola Skoryk, Олександр Миколайович Гнітецький
Cited by: 0
References: 14

Summary

No summary yet. VIRAT can read this paper and write a plain-language summary of its aim, methods, key findings and limitations.

Summarise with VIRAT Free to try with your Science Catalogs account.

Abstract

Purpose. To substantiate and experimentally validate the efficacy of electrolytic purification of kaolin slurry as an alternative to acid bleaching and magnetic separation for the selective extraction of iron- and titanium-bearing chromophore phases, without degrading the aluminosilicate framework of kaolinite Methodology. Raw kaolin was composited and dried for 15 min at 115 °C, after which a working slurry was prepared (250 g dry kaolin per 200 mL water). Electrolysis with direct current was conducted in a glass cell (interelectrode gap 50 mm) at a current of 4 A for 1.5 h. The precipitated products were separated by filtration, washed, dried to constant mass, and subjected to standard chemical analysis. Mean oxide contents and loss on ignition (LOI) were compared between the feed and the upgraded samples. Results. The average Fe₂O₃ content decreased from 0.876% to 0.746%, and TiO₂ from 0.327% to 0.300%. LOI declined, consistent with the removal of hydrated iron compounds. The contents of K₂O and Na₂O changed insignificantly (fluctuations within 3%), whereas Al₂O₃ increased, indicating preservation of the kaolinite matrix. Scientific novelty. The study establishes the viability of a simple, direct-action electrolytic scheme applied to kaolin slurry without prior acid leaching and without magnetic separation. It demonstrates controlled transport and localized precipitation of Fe³⁺/Ti⁴⁺ within the working volume while maintaining the particle-size distribution and the integrity of the principal mineral, enabling selective removal of chromophore phases. Practical significance. The proposed operating regime can serve as a pre-bleaching step in wet beneficiation flowsheets to reduce Fe/Ti levels without introducing aggressive reagents, thereby mitigating corrosion risks and salt–sulfite waste generation. The methodology is technologically compatible with existing equipment and is aimed at improving the optical performance of kaolin by selectively extracting color-inducing phases with minimal loss of the fine clay fraction. Key words: kaolin; electrolysis; iron oxide; titanium oxide; beneficiation.

Fields of Study & Subjects

Extraction and Separation Processes Electrokinetic Soil Remediation Techniques Mineral Processing and Grinding

Publication details

Journal / source
Naukovyi visnyk Donetskoho natsionalnoho tekhnichnoho universytetu
Volume
1
Issue
16
Pages
101–108
Publication date
19 February 2026
Language
EN