Reduction of Sink Mark Defects in Injection Molding of Polyoxymethylene (POM) Through Thermal Modeling and Process Parameter Optimization
Summary
No summary yet. VIRAT can read this paper and write a plain-language summary of its aim, methods, key findings and limitations.
Summarise with VIRAT Free to try with your Science Catalogs account.Abstract
This study aims to minimize sink-mark defects in polyoxymethylene (POM) injection-moulded products through thermal modelling and process parameter optimization. The end-of-packing temperature (TEOP) was estimated using a one-dimensional transient cooling model. At the same time, the specific volume at the end of packing (vEOP) was calculated using the Two-Domain Tait Equation of State. Volumetric (SV) and linear shrinkage (SL) were derived following Chen’s shrinkage framework. Results showed that vEOP ranged from 0.1640 to 0.1764 m³/kg, SV ranged from 13.30 to 19.40%, and SL ranged from 4.64 to 6.94%. Higher TEOP correlated with increased vEOP and higher shrinkage, indicating ineffective packing. Optimization revealed that a melt temperature of 203.41 °C, combined with TEOP of 145.02 °C and a cooling temperature of 16 °C, produced zero shrinkage in the model. These findings provide a quantitative basis for defining process control limits for melt temperature, coolant stability, and packing conditions to reduce sink marks and improve dimensional consistency of POM products.
Fields of Study & Subjects
Injection Molding Process and Properties
Polymer crystallization and properties
Additive Manufacturing and 3D Printing Technologies
Publication details
- Journal / source
- Jurnal Inotera
- Volume
- 11
- Issue
- 1
- Pages
- 161–170
- Publication date
- 28 March 2026
- Language
- EN