In this paper we investigate the use of sucrose as a reducing agent for the carbothermal reduction in spent ternary cathode materials. During this process, lithium from the cathode material is converted into water-soluble Li2CO3, while the high-valent transition metals are reduced to insoluble metallic elements and oxides. The influence of various pyrolysis temperatures, sucrose dosages, and pyrolysis times on the reduction degree of high-valent metals. Furthermore, the influence of leaching conditions on lithium recovery efficiency is examined. Under the optimal conditions of a pyrolysis temperature of 650 °C, a sucrose dosage of 15 wt.%, a pyrolysis time of 30 min, a leaching solid–liquid ratio of 30 g/L, and a leaching time of 30 min, the lithium leaching rate reaches 97.9%. Characterization via XRD, XPS and SEM reveals that sucrose serves as an effective carbothermal reducing agent. It facilitates the reduction of high-valent transition metals to insoluble metallic elements and oxides while simultaneously enabling the recovery of lithium as Li2CO3. Consequently, this method achieves an efficient separation of lithium from other metallic elements. Compared to traditional recycling processes, it avoids the low lithium recovery rates often associated with subsequent separation steps.

Fields of Study & Subjects

Extraction and Separation Processes Recycling and Waste Management Techniques Advancements in Battery Materials

Publication details

Journal / source
Crystals
Publisher
MDPI AG
Volume
16
Issue
5
Pages
341–341
Publication date
18 May 2026
Language
EN