Abstract

The brittleness of 18-karat purple gold originates from the AuAl2 intermetallic compound. This study investigates the microstructural modification of the AuAl2 intermetallic compound by adding silicon (Si) and cobalt (Co) and by rapid solidification in copper molds. The samples with alloy additions from a traditional investment casting were compared with copper mold casting for grain boundary characteristics using SEM, EBSD, and TEM. SEM micrographs showed a reduction in grain size of copper mold casting from approximately within 150–200 μm to within 12–20 μm. EBSD showed a narrow grain size distribution in the Si–Co-modified alloy than in the Si-modified alloy, using the copper mold casting technique. TEM observations show that grain boundaries were closely packed, with ~80 nm-sized voids. XRD confirmed that all alloys retained the AuAl2 intermetallic phase, with peak broadening in the modified and fast-cooling samples indicating crystallographic refinement. These results confirm that Si-Co additions with a fast cooling rate effectively refine the microstructure of the AuAl2 intermetallic compound, making the alloy less brittle while preserving the purple gold color.

Fields of Study & Subjects

Metallurgical and Alloy Processes Intermetallics and Advanced Alloy Properties Aluminum Alloy Microstructure Properties

Publication details

Journal / source
Metals
Volume
16
Issue
3
Pages
355–355
Publication date
23 March 2026
Language
EN