Titanium coatings formed on stainless steel by electrospark deposition in controlled gaseous atmosphere
Summary
No summary yet. VIRAT can read this paper and write a plain-language summary of its aim, methods, key findings and limitations.
Summarise with VIRAT Free to try with your Science Catalogs account.Abstract
The study investigated titanium coatings formed on AISI 304 austenitic stainless steel using electric spark deposition (ESD) at elevated (1140 Torr), normal (760 Torr), and reduced (380 Torr) air or argon pressure, an operating current of 0.5...2.0 A, and a constant electrode-tool travel speed of 60 mm/min. The coatings were characterized by a thickness from (4.2 ± 1.5) to (18.8 ± 9.9) μm, wear resistance class 6, and discharge 3—4. The layers deposited in air were characterized by oxygen content from 12.29 ± 3.6 to 20.09 ± 11.23 % at. and nitrogen from 1.47 ± 2.55 to 4.93 ± 4.84 % at., average splat size from (79.5 ± 48.8) to (210 ± 128.3) μm, microhardness from (5.0 ± 0.26) to (8.25 ± 0.33) GPa. The use of argon environment allowed us to limit the oxygen content within 8.68...15.05 % at., eliminate the nitrogen content, stabilize the average splat size in the range of (72.6...163.8) μm and reduce the microhardness to (4.37...6.38) GPa.
Fields of Study & Subjects
Surface Treatment and Coatings
Electrodeposition and Electroless Coatings
Metal Alloys Wear and Properties
Publication details
- Journal / source
- Strengthening Technologies and Coatings
- Publication date
- 20 February 2026
- Language
- EN