Figure S1 show the top-view and cross-section view of m-Al2O3 layer; Figure S2 show the optical microscope images of Cs₂TeI₆ thick films fabricated by different TMB doping ratios; Figure S3 shows the XRD patterns of Cs₂TeI₆ thick films fabricated by different TMB doping ratios; Figure S4 shows the X-ray response of Cs₂TeI₆ detector exposed to ambient air for 90 days.