Low-temperature Al2O3/ZnO thin-film transistors for 3D heterogeneous integration: interface engineering, bias stress instability, and reliability mechanisms
Summary
No summary yet. VIRAT can read this paper and write a plain-language summary of its aim, methods, key findings and limitations.
Summarise with VIRAT Free to try with your Science Catalogs account.Abstract
Back-end-of-line (BEOL) process scaling and the emergence of three-dimensional heterogeneous integration (3D-HI) demand thin-film transistors (TFTs) that can be integrated within a limited thermal budget while maintaining high electrical performance (µFE > 10 cm2 V−1 s −1 ), long-term reliability (|∆VTH| < 0.5 V after 1 h stress), and low manufacturing cost. Zinc oxide (ZnO) has attracted sustained interest as a channel material owing to its wide bandgap (∼3.3 eV), optical transparency, and compatibility with low-temperature processing. However, the stability of ZnO TFTs remains a major bottleneck, particularly in devices employing atomic-layer-deposited (ALD) aluminium oxide (Al2O3) gate dielectrics, where the dielectric/semiconductor interface critically governs bias-stress degradation. This thesis systematically investigates the interdependence between Al2O3 deposition temperature (150–300 ◦C), interface-trap density (Dit), and bias-stress instability mechanisms in ZnO TFTs. A unified device platform was developed, incorporating both global p-Si bottom gates and patterned AZO bottom gates, enabling separation of intrinsic dielectric effects from gate-geometry-induced field crowding. Cross-sectional transmission electron microscopy (TEM), together with SILVACO/TCAD simulations, confirms the presence of localised electric-field enhancement at wet-etched sharp gate corners, which promotes percolation-type leakage paths and soft breakdown, particularly under high drain bias (VD = 15 V), where threshold-voltage shifts exceeding 1.2 V are observed. A clear trade-off between mobility and reliability is identified as a function of Al2O3 deposition temperature. Devices fabricated with Al2O3 deposited at 150 ◦C exhibit lower field-effect mobility (µFE ≈ 4.8 cm2 V−1 s −1 ) yet the most stable behaviour, with small hysteresis (< 0.2 V) and reduced trap density (Ntrap ∼ 3 × 1012 cm−2 ), consistent with hydrogen-assisted defect passivation. By contrast, films deposited at 300 ◦C are denser and yield higher mobility (µFE ≈ 8.7 cm2 V−1 s −1 ), but suffer from substantially increased hysteresis (> 1.0 V) and higher trap density (Ntrap > 1 × 1013 cm−2 ). Capacitance–voltage (C–V) analysis shows a dielectric constant of k ≈ 8.2 and a stable oxide capacitance (Cox ≈ 7.5 × 10−7 F cm−2 ). Under positive bias stress (PBS, +10 V) in the dark, significant charge trapping is observed with ∆VTH up to +2.3 V, whereas negative bias stress (NBS) in the dark is comparatively weak (∆VTH > −0.2 V), consistent with limited de-trapping dynamics in p-Si gated structures. Optical excitation at 365 nm (photon energy ∼3.4 eV) profoundly alters the stress response through photo-generated carriers. Under illumination, PBS exhibits an initial rapid ∆VTH shift (e.g., ∼ +0.8 V within 60 s), followed by partial saturation consistent with enhanced de-trapping. Conversely, NBS becomes strongly destabilising, producing large negative shifts (e.g., −1.5 V after 1 h) accompanied by marked subthreshold-slope degradation. These results demonstrate that illumination accelerates both trapping and de-trapping processes and highlights the dynamic charge balance at the Al2O3/ZnO interface. By synthesising structural, chemical, and electrical analyses, this thesis establishes a comprehensive reliability map for Al2O3/ZnO TFTs under BEOL-compatible conditions. Three practical design strategies are proposed: (i) gate-geometry engineering to mitigate field crowding and suppress edge-initiated percolation leakage, (ii) interface/dielectric optimisation using lower deposition temperatures (typically ≲ 200 ◦C) to leverage hydrogen-assisted passivation, and (iii) control of plasma chemistry during PEALD to reduce sub-oxide defects. Collectively, these principles provide a pathway to stabilise oxide TFTs for 3D-HI platforms, flexible electronics, and low-power integrated systems.
Fields of Study & Subjects
Thin-Film Transistor Technologies
Semiconductor materials and devices
ZnO doping and properties
Publication details
- Journal / source
- ePrints Soton (University of Southampton)
- Publication date
- 1 March 2026
- Language
- EN
- Document type
- Thesis